DZ445镍基高温合金高温长时间氧化形成的多层膜结构 |
| 刘来娣, 丁彪, 任维丽, 钟云波, 王晖, 王秋良 |
|
Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature |
| LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang |
| 图7 lnK和1 / T的关系图 |
| Fig.7 Logarithm of lnK plotted against the temperature reciprocal (1 / T) before and after the formation of the continuous subouter layer and subinner layer |
|