DZ445镍基高温合金高温长时间氧化形成的多层膜结构 |
| 刘来娣, 丁彪, 任维丽, 钟云波, 王晖, 王秋良 |
|
Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature |
| LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang |
| 图1 DZ445镍基高温合金在900℃氧化不同时间的XRD谱 |
| Fig.1 XRD spectra of the DZ445 Ni-based superalloy after the oxidation at 900oC for different time |
|