镁合金抗高温氧化机理研究进展 |
| 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江 |
|
Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys |
| SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang |
| 图8 Fe-9Cr F-M钢在600℃水蒸气中氧化100 h后的内层氧化物的APT分析[ |
| Fig.8 Atom probe tomography (APT) analyses of cross-sectional oxide film of Fe-9Cr F-M steel after exposure to 600oC steam for 100 h[ (a) APT data set showing the 3D chemical composition distribution in the chromite precipitates and surrounding metal in the internal oxide laye (b) concentration profiles across the chromite-metal interface |
|