镁合金抗高温氧化机理研究进展 |
| 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江 |
|
Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys |
| SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang |
| 图4 Mg-Gd合金在740℃空气中所形成氧化膜的TEM明场像,及立方相、Gd2O3、MgO和基体的HRTEM像[ |
| Fig.4 TEM bright field image of oxide film of Mg-Gd alloy at 740oC (a); HRTEM images of cubic phase (b), Gd2O3 (c), MgO (d), and matrix (e), respectively[ |
|