镁合金抗高温氧化机理研究进展 |
| 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江 |
|
Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys |
| SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang |
| 图1 Mg-Er合金在500℃时反应(3)~(5)的Gibbs自由能变化(ΔG)与Er原子分数的关系[ |
| Fig.1 Relationships between Gibbs free energy change (ΔG)for the reactions (3)-(5) of Mg-Er alloy and atomic fraction of Er at 500oC[ |
|