镁基材料中储氢相及其界面与储氢性能的调控 |
| 李谦, 孙璇, 罗群, 刘斌, 吴成章, 潘复生 |
|
Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance |
| LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng |
| 图4 不同纳米结构Mg的吸氢动力学对比[ |
| Fig.4 Comparisons of hydrogen absorption kinetics of different nanostructured Mg[ |
|