体心立方金属韧脆转变机制研究进展 |
| 韩卫忠, 卢岩, 张雨衡 |
|
Mechanism of Ductile-to-Brittle Transition in Body-Centered-Cubic Metals:A Brief Review |
| HAN Weizhong, LU Yan, ZHANG Yuheng |
| 图5 轧制W板在韧脆转变前后的位错结构[ |
| Fig.5 Dislocation structures in rolled tungsten at different testing temperatures[ (a) pre-existing dislocations before testing (b) below DBTT (c) at DBTT (d) above DBTT |
|