Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr
LI Xin, JIANG He, YAO Zhihao, DONG Jianxin
表1 3种晶界理想拉伸实验结果
Table 1 Ideal strength test results of three kinds of grain boundaries
SystemTensile strength / GPaFracture strain
PureO1O2O3PureO1O2O3
Ni31.5924.7322.7517.430.300.220.280.09
Co34.8928.6924.7125.570.210.140.130.10
NiCr26.2519.6620.3621.030.160.160.170.18