O原子对高温合金基体Ni、Co和NiCr晶界作用的理论计算分析
李昕, 江河, 姚志浩, 董建新

Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr
LI Xin, JIANG He, YAO Zhihao, DONG Jianxin
图9 不同O含量下的Ni晶界的理想分离功差值(Δ)
Fig.9 Differences of separation work (Δ) of Ni grain boundary under different oxidized conditions (IS—effect of interstitial structure, CC—effect of chemical and compressed imputity)