Zr-Sn-Nb-Fe-V合金在过热蒸汽中的周期性钝化-转折行为 |
| 廖京京, 张伟, 张君松, 吴军, 杨忠波, 彭倩, 邱绍宇 |
|
Periodic Densification-Transition Behavior of Zr-Sn-Nb-Fe-V Alloys During Uniform Corrosion in Superheated Steam |
| LIAO Jingjing, ZHANG Wei, ZHANG Junsong, WU Jun, YANG Zhongbo, PENG Qian, QIU Shaoyu |
| 图8 t-ZrO2等效厚度随腐蚀状态参数的变化规律及内表面t-ZrO2特征峰位随腐蚀时间演变 |
| Fig.8 Evolutions of equivalent tetragonal thickness versus corrosion stage parameter (a) and t-ZrO2 peaks versus corrosion time (b) |
|