Zr-Sn-Nb-Fe-V合金在过热蒸汽中的周期性钝化-转折行为 |
| 廖京京, 张伟, 张君松, 吴军, 杨忠波, 彭倩, 邱绍宇 |
|
Periodic Densification-Transition Behavior of Zr-Sn-Nb-Fe-V Alloys During Uniform Corrosion in Superheated Steam |
| LIAO Jingjing, ZHANG Wei, ZHANG Junsong, WU Jun, YANG Zhongbo, PENG Qian, QIU Shaoyu |
| 图5 N2合金腐蚀不同时间后氧化膜内表面SEM像和CLSM三维形貌像 |
| Fig.5 SEM images (a-d) and CLSM 3D images (e-h) of inner-face of N2 alloy corroded for 20 d (T2 = 0.15) (a, e), 60 d (T2 = 0.46) (b, f), 120 d (T2 = 0.92) (c, g), and 140 d (T2 = 1.08) (d, h) |
|