CrFeNi中熵合金在宽温域拉伸条件下的力学行为与变形本构方程 |
| 王凯, 晋玺, 焦志明, 乔珺威 |
|
Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K |
| WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei |
| 图10 不同本构模型对实验数据的描述误差 |
| Fig.10 Description errors of experimental data for each constitutive model (strain rate—description error of experimental data obtained at constant temperatures and different strain rates; temperature—description error of experimental data obtained at constant strain rates and different temperatures; average—description error of all experimental data) |
|