CrFeNi中熵合金在宽温域拉伸条件下的力学行为与变形本构方程
王凯, 晋玺, 焦志明, 乔珺威

Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K
WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei
图9 准静态加载和低温加载下实验数据和基于物理基础的本构模型(ZA、NNL和PB模型)结果的对比
(a, b) ZA model (c, d) NNL model (e, f) PB model
Fig.9 Comparisons of experimental data and physically-based constitutive model description under quasit-static loading (a, c, e) and cryogenic loading (b, d, f)