CrFeNi中熵合金在宽温域拉伸条件下的力学行为与变形本构方程
王凯, 晋玺, 焦志明, 乔珺威

Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K
WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei
图8 准静态加载和低温加载下实验数据和唯象本构模型(JC和KHL模型)结果的对比
Fig.8 Comparisons of experimental data and phenomenological constitutive model description under quasit-static loading (a, c) and cryogenic loading (b, d) (ε˙—strain rate, T—temperature)
(a, b) JC model (c, d) KHL model