CrFeNi中熵合金在宽温域拉伸条件下的力学行为与变形本构方程 |
| 王凯, 晋玺, 焦志明, 乔珺威 |
|
Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K |
| WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei |
| 图7 CrFeNi中熵合金不同温度拉伸断裂后的EBSD带衬度图 |
| Fig.7 EBSD band contrast maps of CrFeNi MEA after tension with Σ3 twin boundary (yellow lines) (a) 77 K (b) 298 K (c) 473 K (d) 673 K (e) 873 K (f) 1073 K |
|