CrFeNi中熵合金在宽温域拉伸条件下的力学行为与变形本构方程
王凯, 晋玺, 焦志明, 乔珺威

Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K
WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei
图3 在应变速率为10-3 s-1及不同变形温度下CrFeNi中熵合金的力学性能
Fig.3 Mechanical properties of CrFeNi MEA at different deformation temperatures and strain rate of 10-3 s-1
(a) quasi-static tensile engineering stress-strain curves
(b) yield stress (YS), ultimate tensile strength (UTS), and uniform elongation (UE)
(c) true stress-strain curves
(d) corresponding work hardening rate-true strain curves