AlCr1.3TiNi2 共晶高熵合金的高温摩擦学性能及磨损机理 |
| 苗军伟, 王明亮, 张爱军, 卢一平, 王同敏, 李廷举 |
|
Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature |
| MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju |
| 图6 Si3N4球与AlCr1.3TiNi2合金和GH4169合金在不同温度下对磨后磨斑区域的SEM二次电子像 |
| Fig.6 SEM secondary electron images of the worn surfaces of Si3N4 ball sliding against AlCr1.3TiNi2 EHEA (a-d) and GH4169 superalloy (a1-d1) at RT (a, a1), 200oC (b, b1), 600oC (c, c1), and 800oC (d, d1) |
|