AlCr1.3TiNi2 共晶高熵合金的高温摩擦学性能及磨损机理 |
| 苗军伟, 王明亮, 张爱军, 卢一平, 王同敏, 李廷举 |
|
Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature |
| MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju |
| 图5 GH4169镍基高温合金(标准热处理态)在不同温度摩擦测试后磨痕表面的SEM二次电子像,及400~800℃摩擦测试后磨痕表面的Raman光谱 |
| Fig.5 SEM secondary electron images of the worn surfaces of the treated GH4169 superalloy tested at 25oC (a), 200oC (b), 400oC (c), 600oC (d), and 800oC (e), and Raman spectra of the worn surfaces for the EHEA after testing at 400-800oC (f) |
|