AlCr1.3TiNi2 共晶高熵合金的高温摩擦学性能及磨损机理 |
| 苗军伟, 王明亮, 张爱军, 卢一平, 王同敏, 李廷举 |
|
Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature |
| MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju |
| 图3 铸态AlCr1.3TiNi2共晶高熵合金和热处理态GH4169高温合金在不同测试温度的摩擦系数曲线,及2种合金在不同温度下的平均摩擦系数与磨损率 |
| Fig.3 Friction coefficient curves of the as-cast AlCr1.3TiNi2 EHEA (a) and treated GH4169 superalloy (b) tested at different temperatures, average friction coefficients (c) and wear rates (d) of the two alloys tested at different temperatures (RT—room temperature) |
|