机械球磨结合粉末冶金制备AZ61超细晶镁合金的组织与性能 |
| 朱云鹏, 覃嘉宇, 王金辉, 马鸿斌, 金培鹏, 李培杰 |
|
Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing |
| ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie |
| 图9 挤压态AZ61镁合金拉伸断口的SEM像 |
| Fig.9 SEM fractographs of extruded AZ61 alloy without (a-c) and with (e, f) mechanical milling, and EDS along the line in Fig.9c (d) |
|