GH3535合金中晶界特征对碲致脆性开裂影响的分形分析 |
| 杨杜, 白琴, 胡悦, 张勇, 李志军, 蒋力, 夏爽, 周邦新 |
|
Fractal Analysis of the Effect of Grain Boundary Character on Te-Induced Brittle Cracking in GH3535 Alloy |
| YANG Du, BAI Qin, HU Yue, ZHANG Yong, LI Zhijun, JIANG Li, XIA Shuang, ZHOU Bangxin |
| 图2 未经晶界工程处理(NS)和经晶界工程处理(GS)样品不同类型晶界的OIM图 |
| Fig.2 Orientation image microscopy (OIM) maps of different types of grain boundaries in Non-GBE (NS) (a) and GBE (GS) (b) specimens (GBE—grain boundary engineering, RGB—random grain boundary) |
|