GH3535合金中晶界特征对碲致脆性开裂影响的分形分析 |
| 杨杜, 白琴, 胡悦, 张勇, 李志军, 蒋力, 夏爽, 周邦新 |
|
Fractal Analysis of the Effect of Grain Boundary Character on Te-Induced Brittle Cracking in GH3535 Alloy |
| YANG Du, BAI Qin, HU Yue, ZHANG Yong, LI Zhijun, JIANG Li, XIA Shuang, ZHOU Bangxin |
| 图1 计盒维数法计算晶界分形维数的示意图 |
| Fig.1 Schematic of the fractal dimension of the grain boundary by the box counting method (η—square box size) |
|