La掺杂P型CeyFe3CoSb12 热电材料及涂层的热电性能 |
| 李斗, 徐长江, 李旭光, 李双明, 钟宏 |
|
Thermoelectric Properties of P-Type CeyFe3CoSb12 Thermoelectric Materials and Coatings Doped with La |
| LI Dou, XU Changjiang, LI Xuguang, LI Shuangming, ZHONG Hong |
| 图9 La0.1Ce0.8Fe3CoSb12块体热电材料焊接后接头区域SEM像和元素分布的线扫描 |
| Fig.9 SEM image of the SPSed bulk La0.1Ce0.8Fe3CoSb12 thermoelectric material joint (a) and the line scan result along line AB in Fig.9a (b) |
|