La掺杂PCeyFe3CoSb12 热电材料及涂层的热电性能
李斗, 徐长江, 李旭光, 李双明, 钟宏

Thermoelectric Properties of P-Type CeyFe3CoSb12 Thermoelectric Materials and Coatings Doped with La
LI Dou, XU Changjiang, LI Xuguang, LI Shuangming, ZHONG Hong
图8 La0.1Ce0.8Fe3CoSb12块体热电材料溅射Al-Ni涂层前后热电性能曲线
Fig.8 Thermoelectric properties curves of the SPSed bulk La0.1Ce0.8Fe3CoSb12 thermoelectric material before and after sputtering Al-Ni coating
(a) Seebeck coefficient (b) electrical resistivity
(c) thermal conductivity (d) thermoelectric figure of merit