La掺杂P型CeyFe3CoSb12 热电材料及涂层的热电性能 |
| 李斗, 徐长江, 李旭光, 李双明, 钟宏 |
|
Thermoelectric Properties of P-Type CeyFe3CoSb12 Thermoelectric Materials and Coatings Doped with La |
| LI Dou, XU Changjiang, LI Xuguang, LI Shuangming, ZHONG Hong |
| 图5 La0.1Ce0.8Fe3CoSb12块体热电材料TEM分析 |
| Fig.5 TEM analyses of the SPSed bulk La0.1Ce0.8Fe3CoSb12 thermoelectric material (a) low-magnification bright-field TEM image (b) enlarged view of boxed region b in Fig.5a (c) bright-field TEM image of grain boundary (d) EDS maps of element distribution for Fig.5c (e) HRTEM image corresponding to region e in Fig.1a (Inset shows the SAED pattern) (f) inverse fast Fourier transformation (IFFT) image using the satellite spots in the inset of Fig.5e (CeSb/( (g) IFFT image using the satellite spots in the inset of Fig.5e (CoSb3/( |
|