La掺杂P型CeyFe3CoSb12 热电材料及涂层的热电性能 |
| 李斗, 徐长江, 李旭光, 李双明, 钟宏 |
|
Thermoelectric Properties of P-Type CeyFe3CoSb12 Thermoelectric Materials and Coatings Doped with La |
| LI Dou, XU Changjiang, LI Xuguang, LI Shuangming, ZHONG Hong |
| 图4 LaxCeyFe3CoSb12块体热电材料热输运性能曲线 |
| Fig.4 Heat transport performance curves of the SPSed bulk LaxCeyFe3CoSb12 thermoelectric material (a) total thermal conductivity (Kt) (b) lattice thermal conductivity (KL) (c) carrier thermal conductivity (Ke) (d) the ratio of KL / Kt |
|