激光熔化沉积TiB2 增强TiAl基合金涂层的组织及力学性能 |
| 王虎, 赵琳, 彭云, 蔡啸涛, 田志凌 |
|
Microstructure and Mechanical Properties of TiB2 Reinforced TiAl-Based Alloy Coatings Prepared by Laser Melting Deposition |
| WANG Hu, ZHAO Lin, PENG Yun, CAI Xiaotao, TIAN Zhiling |
| 图10 磨粒磨损条件下产生的剥落坑的高倍形貌 |
| Fig.10 High power morphology of the spalling pit produced by abrasive particles under abrasive conditions |
|