| Method | Raw material | Deposition rate | Material | Manufacturing | Manufacturing | Subsequent | Applicable |
|---|
| | kg·h-1 | utilization | cost | accuracy | machining | workpiece | | | | rate | | mm | | | | SLM | Mg powder | 0.1-0.2 (low) | 10%-60% | High | 0.05 (high) | Unnecessary | Complex, | | | | (low) | | | | small workpieces | | WAAM | Mg filler | > 2 (high) | 90% (high) | Low | 0.2 (low) | Necessary | General, | | wire | | | | | | large workpieces |
|
|
|