增材制造镁合金技术现状与研究进展 |
| 唐伟能, 莫宁, 侯娟 |
|
Research Progress of Additively Manufactured Magnesium Alloys: A Review |
| TANG Weineng, MO Ning, HOU Juan |
| 图4 SLM过程中镁金属蒸气及样件宏观裂纹现象[ |
| Fig.4 Evaporative fumes during the SLM process of Mg vapor (a) and macro cracks observed on the as built samples (b)[ |
|