Cu-2.0Fe合金等温处理过程中富Fe析出相的形态演变 |
| 陈凯旋, 李宗烜, 王自东, Demange Gilles, 陈晓华, 张佳伟, 吴雪华, Zapolsky Helena |
|
Morphological Evolution of Fe-Rich Precipitates in a Cu-2.0Fe Alloy During Isothermal Treatment |
| CHEN Kaixuan, LI Zongxuan, WANG Zidong, Demange Gilles, CHEN Xiaohua, ZHANG Jiawei, WU Xuehua, Zapolsky Helena |
| 图4 图3中水冷凝固态Cu-2.0Fe合金等温处理后SEM像局部放大图 |
| Fig.4 Magnified SEM images of the square zones in Fig.3 of the isothermal-treated Cu-2.0Fe alloys (a) 924oC, 6 h (b) 964oC, 6 h (c) 984oC, 6 h |
|