SiC颗粒增强Al-Zn-Mg-Cu复合材料的时效行为和力学性能 |
| 马国楠, 朱士泽, 王东, 肖伯律, 马宗义 |
|
Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites |
| MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi |
| 图8 未增强合金和复合材料不同时效处理后晶界的TEM明场像 |
| Fig.8 Bright-field TEM images of grain boundaries of the unreinforced alloy (a, b) and the composite (c, d) (a, c) aging 2 h at 120oC (b, d) T6-treated (120oC, 24 h) |
|