SiC颗粒增强Al-Zn-Mg-Cu复合材料的时效行为和力学性能 |
| 马国楠, 朱士泽, 王东, 肖伯律, 马宗义 |
|
Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites |
| MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi |
| 图5 不同时效状态复合材料沿[110]Al方向的析出相形貌和尺寸统计柱状图 |
| Fig.5 Precipitation morphologies (a-c) and size statistic plots (d-f) of SiC/Al-7.5Zn-2.8Mg-1.7Cu composite under different aging treatment conditions taken along [110]Al zone axis (a, d) under-aged (120oC, 2 h) (b, e) under-aged (120oC, 10 h) (c, f) T6-treated (120oC, 24 h) |
|