SiC颗粒增强Al-Zn-Mg-Cu复合材料的时效行为和力学性能 |
| 马国楠, 朱士泽, 王东, 肖伯律, 马宗义 |
|
Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites |
| MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi |
| 图3 未增强合金和复合材料在120℃下时效0、2、8、10、24和48 h的力学性能 |
| Fig.3 Tensile properties of Al-7.5Zn-2.8Mg-1.7Cu alloy (a) and SiC/Al-7.5Zn-2.8Mg-1.7Cu composite (b) aged at 120oC for 0, 2, 8, 10, 24, and 48 h (UTS—ultimate tensile strength, YS—yield strength, EL—elongation) |
|