共晶高熵合金AlCoCrFeNi2.1 在H2SO4 溶液中的腐蚀行为
胡文滨, 张晓雯, 宋龙飞, 廖伯凯, 万闪, 康磊, 郭兴蓬

Corrosion Behavior of AlCoCrFeNi2.1 Eutectic High-Entropy Alloy in Sulfuric Acid Solution
HU Wenbin, ZHANG Xiaowen, SONG Longfei, LIAO Bokai, WAN Shan, KANG Lei, GUO Xingpeng
表2 AlCoCrFeNi2.1 EHEA的EIS拟合参数
Table 2 Fitted electrochemical parameters for EIS of AlCoCrFeNi2.1 EHEA
SolutionRs / (Ω·cm2)Qdl / (Ω-1·cm-2·s n )nRct / (Ω·cm2)L / (H·cm2)RL / (Ω·cm2)
0.05 mol·L-1 H2SO413.009.8442 × 10-50.8739308.5120.867.22
0.05 mol·L-1 H2SO4 + 0.02 mol·L-1 NaCl17.621.6432 × 10-40.8858271.318.037.70