固态相变对Fe-Co-Ni超高强度钢长臂梁构件焊接-淬火过程应力和变形的影响 |
| 张开元, 董文超, 赵栋, 李世键, 陆善平 |
|
Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes |
| ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping |
| 图12 长臂梁真空气淬冷却过程组织与变形曲线 |
| Fig.12 Phase transformation contour (a) and deformation curves of different positions 1 (b) and 3 (c) in Fig.12a during cooling stage of vacuum gas quenching (Insets in Figs.12b and c show the locally enlarged curves) |
|