固态相变对Fe-Co-Ni超高强度钢长臂梁构件焊接-淬火过程应力和变形的影响 |
| 张开元, 董文超, 赵栋, 李世键, 陆善平 |
|
Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes |
| ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping |
| 图11 长臂梁真空气淬变形云图及底部支撑位置真空气淬变形的模拟结果与实测结果对比 |
| Fig.11 Deformation contour in the component (a) and the comparisons between the experimental and simulated results after vacuum gas quenching at bottom support positions SP1-SP5 (b) |
|