固态相变对Fe-Co-Ni超高强度钢长臂梁构件焊接-淬火过程应力和变形的影响 |
| 张开元, 董文超, 赵栋, 李世键, 陆善平 |
|
Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes |
| ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping |
| 图9 不考虑固态相变的长臂梁真空气淬变形云图 |
| Fig.9 Distortion contours for 0 s (a), 204 s (b), 804 s (c), 2004 s (d), and 4500 s (e) without considering solid-state phase transformation (SSPT) |
|