Macrosegregation Mechanism of Primary Silicon Phase in Cast Hypereutectic Al-Si Alloys Under Alternating Electropulsing |
| ZHANG Limin, LI Ning, ZHU Longfei, YIN Pengfei, WANG Jianyuan, WU Hongjing |
| 图8 电脉冲下初生Si梯度偏析形成的物理模型 |
| Fig.8 Formation model of gradient macro segregation of primary Si phase under electropulsing (F, Fy —electromagnetic repulsive force and its component in y-direction; v —velocity; vx, vy —velocity in x- or y-direction, respectively) (a) the first segregation layer (b) the second segregation layer (c) the third segregation layer (d) near eutectic structure |
|