固态相变和软化效应对超高强钢焊接残余应力的影响 |
| 王重阳, 韩世伟, 谢峰, 胡龙, 邓德安 |
|
Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel |
| WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean |
| 图10 焊接温度循环计算结果和实验结果对比 |
| Fig.10 Comparison of computational results and experimental (Exp.) results of welding temperature cycles (Inset shows the locations of P1 and P2 in the FEM) |
|