冷却速率对管线钢中非金属夹杂物成分演变的影响
|
张月鑫, 王举金, 杨文, 张立峰
|
Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel
|
ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng
|
|
表1 Al、 Mg、Ca、S、O在液态、δ和γ钢中的扩散系数[26~28]
|
Table 1 Diffusion coefficients of dissolved Al, Mg, Ca, S, and O in liquid, δ, and γ steel[26-28]
|
|
Element | In liquid | In δ | In γ |
---|
Al | 3.5 × 10-09 | 5.9 × exp(-241186 / (RT )) / 10000 | 5.15 × exp(-245800 / (RT )) / 10000 | Mg | 3.5 × 10-09 | 0.76 × exp(-224430 / (RT )) / 10000 | 0.055 × exp(-249366 / (RT )) / 10000 | Ca | 3.5 × 10-09 | 0.76 × exp(-224430 / (RT )) / 10000 | 0.055 × exp(-249366 / (RT )) / 10000 | S | 4.1 × 10-09 | 4.56 × exp(-214639 / (RT )) / 10000 | 2.4 × exp(-223426 / (RT )) / 10000 | O | 2.7 × 10-09 | 0.0371 × exp(-96349 / (RT )) / 10000 | 5.75 × exp(-168454 / (RT )) / 10000 |
|
|
|