冷却速率对管线钢中非金属夹杂物成分演变的影响 |
| 张月鑫, 王举金, 杨文, 张立峰 |
|
Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel |
| ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng |
| 图9 不同直径夹杂物成分随着冷却速率的变化 |
| Fig.9 Variations of the composition of inclusions with diameters of 1 μm (a), 2 μm (b), 5 μm (c), and 7 μm (d) with cooling rates |
|