冷却速率对管线钢中非金属夹杂物成分演变的影响 |
| 张月鑫, 王举金, 杨文, 张立峰 |
|
Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel |
| ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng |
| 图8 夹杂物成分随着冷却速率和夹杂物直径的变化 |
| Fig.8 Variations of the composition of inclusions with the cooling rates and their diameters (a) CaO (b) CaS (c) Al2O3 (d) MgO |
|