| 图6 管线钢凝固冷却过程中物相的转变和夹杂物热力学平衡成分随温度的变化 |
| Fig.6 Evolutions of phase (a) and thermodynamic composition of inclusions (b) in the pipeline steel over temperature during steel solidification and cooling (w(i)—mass fraction of element i, T.—total, l—liquid, s—solid) |
|