冷却速率对管线钢中非金属夹杂物成分演变的影响 |
| 张月鑫, 王举金, 杨文, 张立峰 |
|
Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel |
| ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng |
| 图3 不同冷却速率下夹杂物平均成分的变化 |
| Fig.3 Variations of average composition of inclusions at different cooling rates |
|