新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能 |
||||||||||||
| 芮祥, 李艳芬, 张家榕, 王旗涛, 严伟, 单以银 | ||||||||||||
|
Microstructure and Mechanical Properties of a Novel Designed 9Cr-ODS Steel Synergically Strengthened by Nano Precipitates |
||||||||||||
| RUI Xiang, LI Yanfen, ZHANG Jiarong, WANG Qitao, YAN Wei, SHAN Yiyin | ||||||||||||
| 表1 MX相与纳米氧化物对屈服强度的贡献 |
||||||||||||
| Table 1 Contributions of MX precipitates and nano-oxides to yield strength, respectively |
||||||||||||
|
||||||||||||