新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能 |
| 芮祥, 李艳芬, 张家榕, 王旗涛, 严伟, 单以银 |
|
Microstructure and Mechanical Properties of a Novel Designed 9Cr-ODS Steel Synergically Strengthened by Nano Precipitates |
| RUI Xiang, LI Yanfen, ZHANG Jiarong, WANG Qitao, YAN Wei, SHAN Yiyin |
| 图8 不同热处理的新型MX-ODS钢的显微硬度 |
| Fig.8 Dependence of microhardness on heat treatments for the novel MX-ODS steel (a) normalizing temperature (b) tempering temperature |
|