新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能 |
| 芮祥, 李艳芬, 张家榕, 王旗涛, 严伟, 单以银 |
|
Microstructure and Mechanical Properties of a Novel Designed 9Cr-ODS Steel Synergically Strengthened by Nano Precipitates |
| RUI Xiang, LI Yanfen, ZHANG Jiarong, WANG Qitao, YAN Wei, SHAN Yiyin |
| 图6 新型MX-ODS钢中析出相扫描透射电镜高角环形暗场(STEM-HAADF)像及EDS面扫描图 |
| Fig.6 Scanning transmission electron microscopy equipped with high angular annular dark field (STEM-HAADF) image and EDS element maps of V, N, Y, O, and Ta in the novel MX-ODS steel (The rectangular boxes show VN precipitates, and the cycles show Y-Ta-O precipitates; heat treatment: normalizing at 1100oC for 1 h and tempering at 750oC for 1 h) |
|