新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能 |
| 芮祥, 李艳芬, 张家榕, 王旗涛, 严伟, 单以银 |
|
Microstructure and Mechanical Properties of a Novel Designed 9Cr-ODS Steel Synergically Strengthened by Nano Precipitates |
| RUI Xiang, LI Yanfen, ZHANG Jiarong, WANG Qitao, YAN Wei, SHAN Yiyin |
| 图2 基于材料实测化学成分(Fe-8.82Cr-0.99W-0.96Mn-0.39V-0.097Ta-0.12N)的Jmat Pro热力学计算 |
| Fig.2 Thermodynamic calculation according to measured chemical compositions (Fe-8.82Cr-0.99W-0.96Mn-0.39V-0.097Ta-0.12N) (a) relationship between equilibrium phase and temperature (Inset is the local magnified curve) (b) dependence of carbon content on M23C6 amount |
|