基于不同 α / β 团簇式比例的Ti-Al-V合金的铸态组织和力学性能 |
| 朱智浩, 陈志鹏, 刘田雨, 张爽, 董闯, 王清 |
|
Microstructure and Mechanical Properties of As-Cast Ti-Al-V Alloys with Different Proportion of α / β Clusters |
| ZHU Zhihao, CHEN Zhipeng, LIU Tianyu, ZHANG Shuang, DONG Chuang, WANG Qing |
| 图9 铸态Ti-Al-V钛合金的Vickers硬度和密度以及比硬度和比强度 |
| Fig.9 Vickers hardnesses (a), mass densities (b), specific hardnesses (c), and specific strengthes (d) of Ti-Al-V alloys (Specific hardness denotes the hardness-over-density ratio, and specific strength denotes the ultimate tensile strength-over-density ratio, respectively) |
|