基于不同 α / β 团簇式比例的Ti-Al-V合金的铸态组织和力学性能
朱智浩, 陈志鹏, 刘田雨, 张爽, 董闯, 王清

Microstructure and Mechanical Properties of As-Cast Ti-Al-V Alloys with Different Proportion of α / β Clusters
ZHU Zhihao, CHEN Zhipeng, LIU Tianyu, ZHANG Shuang, DONG Chuang, WANG Qing
图2 Ti-Al-V成分图,包含了设计成分、α-[Al-Ti12]Al1Ti2相成分式和部分β相成分式,其中所设计合金分布于连接α-Al2Ti14和β-Al1Ti15V2的直线上(红色方块)
Fig.2 Ti-Al-V ternary composition chart, where are marked the compositions of the designed series, α-[Al-Ti12]Al1Ti2, and some β formulas. The resigned alloy series lie along the straight line (in red) linking α-Al2Ti14 and β-Al1Ti15V2